Mechanical and optical properties of monolithic CAD-CAM restorative materials

dc.authorid0000-0003-4917-4899
dc.contributor.authorŞen, Nazmiye
dc.contributor.authorÖlçer Us, Yeşim
dc.date.accessioned2020-07-21T07:59:15Z
dc.date.available2020-07-21T07:59:15Z
dc.date.issued2018
dc.departmentİstanbul Medipol Üniversitesi, Diş Hekimliği Fakültesi, Protetik Diş Tedavisi Ana Bilim Dalı
dc.description.abstractStatement of problem: Achieving natural tooth appearance with sufficient mechanical strength is one of the most challenging issues of computer-assisted design and computer-assisted manufacturing (CAD-CAM) materials. However, limited evidence is available regarding their optical and mechanical properties for proper and evidence-based material selection in clinical practice.Purpose: The purpose of this in vitro study was to assess and compare the translucency and biaxial flexural strength of 5 monolithic CAD-CAM restorative materials.Material and methods: Disk-shaped specimens (n=30) of each material (Lava Ultimate [LU], Vita Enamic [VE], Vitablocs Mark II [VMII], Vita Suprinity [VS], and IPS e.max CAD [IPS]) with a diameter of 12 mm and a thickness of 1.2 ±0.05 mm were prepared. A spectrophotometer was used to measure the translucency parameter. The specimens were then subjected to a biaxial flexure test using 3 balls and loaded with a piston in a universal testing machine at a cross-head speed of 0.5 mm/min until failure occurred (International Organization for Standardization standard 6872). Weibull statistics were used to evaluate the characteristic strength and reliability of each material. Chemical compositions were analyzed using an energy dispersive spectrometer, and microstructural analysis was conducted using scanning electron microscopy. Data were analyzed using 1-way ANOVA and the Tukey honest significant difference test (?=.05).Results: Significant differences were found among the materials concerning translucency and biaxial flexural strength (P<.05). The highest mean transparency value was obtained in the VS group, whereas the lowest mean value was obtained in the VE group. The VS group produced the highest mean biaxial flexural strength, followed by the IPS, LU, VE, and VMII groups.Conclusions: Based on the results of the present study, zirconia-reinforced glass-ceramic revealed higher mean translucency and biaxial flexural strength than resin nanoceramic, feldspathic ceramic, lithium disilicate ceramic, and dual-network ceramic.
dc.identifier.citationŞen, N. ve Ölçer Us, Y. (2018). Mechanical and optical properties of monolithic CAD-CAM restorative materials. Journal of Prosthetic Dentistry, 119(4), 593-599. https://dx.doi.org/10.1016/j.prosdent.2017.06.012
dc.identifier.doi10.1016/j.prosdent.2017.06.012
dc.identifier.endpage599
dc.identifier.issn0022-3913
dc.identifier.issn1097-6841
dc.identifier.issue4
dc.identifier.scopusqualityQ1
dc.identifier.startpage593
dc.identifier.urihttps://dx.doi.org/10.1016/j.prosdent.2017.06.012
dc.identifier.urihttps://hdl.handle.net/20.500.12511/5584
dc.identifier.volume119
dc.identifier.wosqualityQ2
dc.indekslendigikaynakWeb of Science
dc.indekslendigikaynakScopus
dc.indekslendigikaynakPubMed
dc.language.isoen
dc.publisherElsevier Inc.
dc.relation.ispartofJournal of Prosthetic Dentistryen_US
dc.relation.publicationcategoryMakale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanı
dc.rightsinfo:eu-repo/semantics/openAccess
dc.subjectMonolithic CAD-CAM
dc.subjectRestorative Materials
dc.subjectOptical Properties
dc.titleMechanical and optical properties of monolithic CAD-CAM restorative materials
dc.typeArticle

Files

Original bundle

Now showing 1 - 1 of 1
Loading...
Thumbnail Image
Name:
Olcer Us, Yesim-2017.pdf
Size:
1,014.08 KB
Format:
Adobe Portable Document Format
Description:
Tam Metin / Full Text

License bundle

Now showing 1 - 1 of 1
Loading...
Thumbnail Image
Name:
license.txt
Size:
1.44 KB
Format:
Item-specific license agreed upon to submission
Description: